Failure investigations of a 900 KV bil trench cota bushing

A case study of failure discussed in the 82 nd International Conference of Doble Clients.

bushingThe discussion of this paper will focus on the H1 Trench COTA bushing, which failed after field maintenance handling that would not normally be expected to have a negative effect on a bushing. Following the failure, the top air side porcelain was found ruptured and missing; the bottom insulator was fractured into a number of pieces. The H2 and H3 bushings from this transformer, which were identical Trench type bushings, were also removed and disassembled for inspection to help identify a possible root cause of the H1 bushing failure.

More at : http://www.doble.com/content/show/boston2015/files/BIIT/BIIT-2_Trench_COTA_Failure_Root_Cause_Mani.pdf