Corrosion properties of AISI 321 stainless steel

The main aim of this study was to analyze the pitting corrosion and stress corrosion cracking which is initiated on prototype cold-formed outer exhaust sleeves during the testing of different cleaning procedures before chromium plating. Various microscopic methods were used to identify the initiation of corrosion and its propagation.

  • Severe corrosion occurred in the cleaning solution containing H2SO4 at elevated temperature.
  • Pitting corrosion has formed on the titanium nitride inclusions.
  • Stress corrosion cracking was caused by deformation martensite.

Read this article →

Corrosion cracking of 304L stainless steel pipe clamps

Case study of stainless steel components of a geothermal heating system failed prematurely. The crack surfaces were brittle in appearance and were predominately transgranular. The failure was determined to be caused by chloride induced stress corrosion cracking. Subsequent failures may be avoided by informed alloy selection.

More informations : Transgranular stress corrosion cracking of 304L stainless steel pipe clamps in direct use geothermal water heating applications.

Failure analysis of stress corrosion cracking in a gas transmission steel pipeline

Engineering Failure Analysis : Failure analysis of stress corrosion cracking occurred in a gas transmission steel pipeline

Abstract

In January 2010, stress corrosion cracking was occurred in a high-pressure gas pipeline steel in northern regions of Iran, after almost 40 years since its installation. In this study, failure mechanisms were determined based on available documents and metallographic studies conducted on this pipeline. The results showed that the applied polyethylene tape coating on the external surface of the pipeline became opened and disbonded in the corroded area causing external surface of buried pipeline to be exposed to wet soil around it. As a result of the chemical interactions and formation of carbonate/bicarbonate solution and with the presence of tensile stresses, stress corrosion cracking occurred in the longitudinal direction and at the outer surface of the pipe. In addition, mechanisms and morphology of cracks propagation due to stress corrosion cracking to internal side of the pipe wall were studied.

Keywords: API 5L X60; Stress corrosion cracking; Pipeline; Intergranular