Fatigue cracking of high pressure oil tube

1-s2-0-s2213290213000321-gr1An article about a Case study of failure analysis published in « Case Studies in Engineering Failure Analysis« , July 2013.

A high pressure oil tube with nominal diameter 50.8 mm and nominal thickness 4 mm has prematurely failed with a longitudinal crack. The failure was detected after 11 months of operation. The tube is part of the hydraulic power unit of an off shore oil and gas platform. The maximum designed internal pressure was 20 MPa and the service temperature was 25 °C with no significant variation. In practice, the internal pressure varies from 16 to 20 MPa under operation, and shutdowns rarely occur.

Read more

Publicités

Laisser un commentaire

Entrez vos coordonnées ci-dessous ou cliquez sur une icône pour vous connecter:

Logo WordPress.com

Vous commentez à l'aide de votre compte WordPress.com. Déconnexion / Changer )

Image Twitter

Vous commentez à l'aide de votre compte Twitter. Déconnexion / Changer )

Photo Facebook

Vous commentez à l'aide de votre compte Facebook. Déconnexion / Changer )

Photo Google+

Vous commentez à l'aide de votre compte Google+. Déconnexion / Changer )

Connexion à %s