Stress corrosion cracking of full sized rockbolts

2016-06-04_07h48_16An article published in  « International Journal of Rock Mechanics & Mining Sciences – 81 (2016)« .

Previous studies had identified that a testing protocol was required to examine stress corrosion cracking (SCC) of full sized rockbolts under simulated in situ conditions. It was found that SSR testing provided an appropriate analogue for examining rockbolt susceptibility to SCC and was thus used to examine the effect of grit blasting, galvanising and varying steel grades on the SCC resilience of rockbolts. Of these, 300 grade steel and galvanising provided the most promising resistance to SSC, while grit blasting provided a 40% improvement in resistance compared to untreated HSAC 840 grade rockbolts.

More

Votre commentaire

Entrez vos coordonnées ci-dessous ou cliquez sur une icône pour vous connecter:

Logo WordPress.com

Vous commentez à l’aide de votre compte WordPress.com. ( Déconnexion /  Changer )

Photo Google

Vous commentez à l’aide de votre compte Google. ( Déconnexion /  Changer )

Image Twitter

Vous commentez à l’aide de votre compte Twitter. ( Déconnexion /  Changer )

Photo Facebook

Vous commentez à l’aide de votre compte Facebook. ( Déconnexion /  Changer )

Connexion à %s